Por favor, use este identificador para citar o enlazar este ítem: http://dspace.espoch.edu.ec/handle/123456789/13097
Registro completo de metadatos
Campo DC Valor Lengua/Idioma
dc.contributor.advisorPuente Guijarro, César Arturo-
dc.contributor.authorOcles Morales, Jessica Liliana-
dc.date.accessioned2019-11-13T16:43:58Z-
dc.date.available2019-11-13T16:43:58Z-
dc.date.issued2019-07-08-
dc.identifier.citationOcles Morales, Jessica Liliana. (2019). Rediseño del sistema de tratamiento de aguas residuales para la recuperación de cromo y oxidación de sulfuros en la Curtiembre Pieles Puma de la ciudad de Ambato. Escuela Superior Politécnica de Chimborazo. Riobamba.es_ES
dc.identifier.urihttp://dspace.espoch.edu.ec/handle/123456789/13097-
dc.descriptionSe rediseñó el sistema de tratamiento de aguas residuales para reducir los sulfuros del agua de pelambre y recuperar el cromo III del agua del proceso de curtido para su posterior reutilización. En este trabajo se establecieron tres etapas: Primera etapa, la caracterización de las aguas de los diferentes procesos, en las que se determinan valores fuera de la normativa para aguas de pelambre como: demanda química de oxígeno, demanda bioquímica de oxígeno y sulfuros; para aguas del proceso de curtido, parámetros fuera de norma como: demanda química de oxígeno, demanda bioquímica de oxígeno y Cromo hexavalente. Segunda etapa; ejecución de las pruebas experimentales de coagulación-floculación, en las siguientes condiciones: concentración de policloruro de aluminio (PAC) de 20 mg/L para aguas de curtido y 40 mg/L en aguas de pelambre, con pH de 9. Posteriormente se realiza la sedimentación, aireación y filtración. Tercera etapa; precipitación de Cromo III en presencia de ácido sulfúrico (1:10) con pH aproximado de 3. Como resultado, en aguas de pelambre se obtuvo un porcentaje de remoción para: sulfuros igual a 95,9%, demanda química de oxígeno igual a 91,8%, demanda bioquímica de oxígeno igual a 99,3%, mientras que para aguas de curtido se obtuvieron porcentajes de remoción para: Cromo total igual a 99,8%, demanda química de oxígeno igual a 79,5%, demanda bioquímica de oxígeno igual a 97,5%. Con el Cromo III reciclado implementado en el proceso de curtido al 30% se obtuvieron pieles a las que se realizaron las siguientes pruebas físicas: Resistencia a la tensión con medias de 1461,48 N/cm2; Porcentaje de elongación, un promedio de 63,75%; Lastometría, valor medio de 9,52 mm. Se concluyó que el Cromo reciclado en este porcentaje dio buenas propiedades físicas al cuero. Se recomienda implementar el sistema de tratamiento de aguas residuales, evitando descargar el agua contaminada proveniente de las etapas de curtido y pelambre.es_ES
dc.description.abstractThe wastewater treatment system was redesigned to reduce the sulphides of the hair water and to recover the chromium III from the water of the tanning process for its subsequent reuse. In this work, three stages were established: First stage, the characterization of the waters of the different processes, in which values outside the regulations are determined for wastewater such as: chemical oxygen demand, biochemical demand of oxygen and sulphides; for waters of the tanning process, out of standard parameters such as: chemical oxygen demand, biochemical oxygen demand and hexavalent chromium. Second stage; execution of the experimental coagulation-flocculation test, under the following conditions: concentration of aluminium polychloride (PAC) of 20 mg/L for tanning waters and 40 mg/L in waters of hair, with a pH of 9. It is then carried out sedimentation, aeration and filtration. Third stage; precipitation of Chromium III in the presence of sulfuric acid (1:10) with an approximate pH of 3. As a result, in scrub waters a removal percentage was obtained for: sulphides equal to 95,9%, chemical oxygen demand equal to 91,8%, oxygen biochemical demand equal to 99,3%, while for tanning waters removal percentages were obtained for: Total chromium equal to 99,8%, chemical oxygen demand equal to 79,5%, biochemical oxygen demand equal to 97,5%. With the recycled chromium III implemented in the tanning process at 30%, skins were obtained to which the following physical tests were carried out: Resistance to tension with averages of 1461,48 N/cm2; Elongation percentage, an average of 63,75%; Lastometry, average value of 9,52 mm. It was concluded that the recycled chromium in this percentage gave good physical properties to the leather. It is recommended to implement the wastewater treatment system, avoiding the discharge of contaminated water from the tanning and furling stages.es_ES
dc.language.isospaes_ES
dc.publisherEscuela Superior Politécnica de Chimborazoes_ES
dc.relation.ispartofseriesUDCTFC;96T00550-
dc.rightsinfo:eu-repo/semantics/openAccesses_ES
dc.subjectINGENIERÍA Y TECNOLOGÍA QUÍMICAes_ES
dc.subjectLASTOMETRÍAes_ES
dc.subjectRESISTENCIA A LA TENSIÓNes_ES
dc.subjectPORCENTAJE DE ELONGACIÓNes_ES
dc.subjectTRATAMIENTO FÍSICOes_ES
dc.subjectCROMO RECICLADOes_ES
dc.subjectSULFUROSes_ES
dc.titleRediseño del sistema de tratamiento de aguas residuales para la recuperación de cromo y oxidación de sulfuros en la Curtiembre Pieles Puma de la ciudad de Ambato.es_ES
dc.typebachelorThesises_ES
dc.contributor.miembrotribunalTapia González, Zoila Valeria-
dc.rights.urihttps://creativecommons.org/licenses/by-nc-sa/3.0/ec/es_ES
Aparece en las colecciones: Ingeniero/a Químico/a

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
96T00550.pdf5,52 MBAdobe PDFVista previa
Visualizar/Abrir


Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons Creative Commons